作者swaidatol (教练谢谢您)
看板Master_D
标题[请益] 不好意思
时间Mon Jan 8 00:18:54 2007
这几天在准备报告 所以问了很多问题 请见谅
我找的paper实验的地方我是有看没有懂
各个单字翻译过也都ok 但是凑起来就不是那麽一回事
由於是实验的地方 所以小心谨慎一点的好
不知有没有人能帮我翻译一下我好对照我自己翻的狗屁不通的怪东西
The binary Nb-Ti couples were first prepared by diffusion welding the
elemental bars in a silica capsule back-filled with high purity argon at
1100 度C for 72 h. One of the Nb-Ti couples and a Si block were ground,
polished, cleaned, and then swathed together with Mo wires to make a Nb-Ti-Si
diffusion couple, which was wrapped in Mo foil. Three well-prepared Nb-Ti-Si
diffusion couples were sealed in a silica capsule back-filled with high
purity argon, and annealed in an L4514-type diffusion furnace (Qingdao
Instrument and Equipment Co. Ltd., China) at 1000 ± 1度 C for 440 h. After
completion of annealing, the samples were quenched in water.
The alloys were prepared by arc melting pure elements in an arc furnace under
argon at- mosphere using a non-consumable tungsten electrode. The buttons
were remelted 6 times to improve their homogeneity.
以上这2段实验步骤 字义都不困难 但我就是不能把他的步骤连贯起来(2段分开)
希望有强者能帮帮我 我卡很久了 谢谢!!
--
○ 给我趴好!
√\\
--
※ 发信站: 批踢踢实业坊(ptt.cc)
◆ From: 61.230.209.180
1F:→ afunism:连不起来的话....用条列式表示不是也容易让人看懂? 01/08 15:06